Offset printing l Double-Layered UV-CTP (CTcP) |
Printopia
UPLUX 4UV CTcP Plate, a mighty design as a CTcP system for an excellent resistance of UV inks, with the latest double layer coating technology. With the latest
double layer coating technology, it provides both advantages of
high sensitiveness and good productivity.
Features l Printopia UPLUX 4UV CTcP Plate |
- Consistent quality, solid reliability and wide latitude.
Parameter adjustment is not really needed. Printopia UPLUX 4UV is very easy for your machines and chemicals to adapt.
- Greater resistance to chemicals and scratches
Especially to alkaline and alcohol, to protect the plates from chemical
- Even electrochemical-grained substrate
Besides AGFA, FUJI, KODAK, we trim (cut the edge of) the plates to make it better and stabilize the operation process.
- Extensive adaptability
Being adapted to most of the platesetters, processors and developers.
Please directly contact us for detailed catalog.
Offset Printing Plate ∣ Common size (mm)
|
1030 X 770
|
1030 X 785
|
1030 X 790
|
1030 X 795
|
1030 X 800
|
915 X 715
|
925 X 740
|
745 X 605
|
670 X 560
|
650 X 550
|
510 X 400
|
450 X 370 |
Offset Printing l Articles and Video |
- Youtube Video -
- Article -
Printopia UPLUX 4UV l Double-Layered UV-CTP (CTcP) |
Please directly contact us for detailed technical date sheet for processing with our plates.
Plate Type |
- Double Layer/coating printing plate
- Positive-working CTcP plate with optional post-bake for longer runs
|
Thickness / Gauge |
0.15 / 0.20 / 0.25 / 0.30 / 0.40 mm |
Colour |
Blue colour |
Shelf Life |
18 months under standard storage conditions |
Substrate |
electro-chemically grained and anodized lithographic aluminum |
Compatible Platesetter |
All the common platesetter brands in the market |
Operation Term |
Imaging
|
Safelight |
Handling under UV-free yellow safelight |
Spectral Sensitivity |
360-420nm |
Exposure Energy |
50 mJ/ cm² |
Resolution |
1-99% @ 250lpi |
FM Capability |
10 micron stochastic |
Processing
|
Developer |
Printopia Developer or other common brands in market. |
Developer Dilution |
1:4 recommended |
Replenishing Rate |
60ml/ m² |
Processing Temperature |
24-26 ℃ |
Processing Dwell Time |
20-30 seconds |
On-press
|
Run Length |
- 150,000-250,000 impressions (Normal-ink unbaked)
- 100,000 - 150,000 impressions (UV-ink unbaked)
- Above 1,000,000 impressions (baked)
- Actual run length may vary according to press, ink, and paper conditions
|
Plate Baking |
220 ℃ for 8-15 minutes |
Storage Conditions |
- Keep flat and away from immoderate cold, heat and humidity
- Controlled enviroment temperature 15 to 25℃, relative humidity 60%
|